PROCESS FOR ALUMINIUM
  Process
Compositions & Operating Conditions.
Applications & Features
       
ALOBOND DIP Concentration 500 ml/l Produces a light grey deposit on aluminium a nickel strike is recommended after
AL - 44 Temperature Room
  Time 1-2 mins.
TECHNICAL DATA      