GOLD PLATING PROCESS
  Process
Compositions & Operating Conditions.
Applications & Features
       
NEUTRAL P & C BATH Gold Makeup 1000 100 ml/l It gives 22-24k fash coating with Uniform thickness mainly used artificial jewellery, spectacles, watch cases the process is easy to hadle.
  Gold Makeup 1001 20 ml/l
  Gold Brightner 1002 100 ml/l
  Voltage 6-8 V
  Temperature 50-60 ° C
  Plating time 10-20 sec.
  pH 7-Aug  
  Anodes 316 S.S  
  Agitation Article Movement.  
TECHNICAL DATA      
» Download        
       
ALKALINE GOLD PROCESS Concentration 100 ml/l The bath is mainly used to produce alloy plating with gold to achieve different colours i.e. green, pink, white.
  Temperature 40-50 ° C
  Rod movement Required
  Voltage 4-5 volts
  Anodes 316 S.S
TECHNICAL DATA      
» Download