Process | Compositions& Operating Conditions | Applications & Features | |
AURO FLASH MAKE UP | AURO FLASH CONC. Gold brightener 1002 Voltage Temperature Plating time pH Anodes Agitation Gold contents (reqd.) |
100 ml/l 100 ml/l 6-8 V 50-60°C 10-20 sec. 6.5-7.5 316 S.S Article Movement. 0.5-1 gm/l |
It gives 24k flash coating with Uniform thickness mainly used in artificial jewellery, spectacles, watch cases the process is easy to operate. |
AURO ALKALINE PROCESS | Concentration Temperature Rod movement Voltage Anodes Gold contents (reqd.) |
100 ml/l 40-50°C Required 4-5 volys 316 S.S 0.5-1 gm/l |
The bath is mainly used to produce alloy plating with gold to achieve different colours i.e. green, pink, white. |
ALKALINE GOLD ADDITIVES TO PRODUCE DIFFERENT GOLD COLOURS | 1K Addditive 2K Addditive 3K Addditive 4K Addditive 5K Addditive |
Whitish Deposit Light Yellow Reddish Brown Dark Gold Pink Gold Deposit Light Greenish Deposit |
MICRON GOLD PLATING PROCESS
Process | Compositions& Operating Conditions | Applications & Features | |
AURO MICRON MAKE UP | Makeup Solution
|
Ready to use
1 ml for 1gm Gold Metal |
Gives very bright Hamilton gold finish for plating on jewellery, spectacle frames, wrist watches, The deposit is app. 23.5 Karat having a hardness of around 200 - 220 vickers. Gives very bright rich gold finish for plating on jewellery, spectacle frames, wrist watches & sanitary fitting. |