DULL NICKEL
Process | Compositions& Operating Conditions | Applications & Features | |
DULL NICKEL | Dull Nickel Salt NS-68 Nickel Additive - 512 Temperature pH |
150-250 g/l 4-6 ml/l 40-50°C 4.8-5.1 |
Used for dull nickel plating or semi bright nickel plating usually called as peuter plating process gives dull grey finish mostly used on zinc based ,deposit is slow. |
BRIGHT NICKEL
Process | Compositions& Operating Conditions | Applications & Features | |
NICKEL BRIGHTENER 986 | Bright Nickel Salt Nickel Additive 512/502 Nickel Brightener 986 Temperature pH Cathode current density |
350-375 g/l 10 ml/l 0.6-1 ml/l 55-60°C 4.6-5.1 3-4 A/dm² |
Produces mirror bright finish on zinc based die casting, plastics and brass easy maintenance. Very good tolerance to variation in temperature and bath concentrations excellent chrome receptivity very good low current density brightness suitable for vat and barrel plating veryeconomical process. |
NICKEL BRIGHTENER 1286/2586 | Bright Nickel Salt Nickel Additive 512/502 Nickel Brightener 1286/2586 Temperature pH Cathode current density |
350-375 g/l 10 ml/l 0.3-0.6 ml/l 55-60°C 4.6-5.1 3-4 A/dm² |
Produces mirror bright finish on mild steel and stainless steel. high levelling brightener system. |
NICKEL BRIGHTENER 5047 | Bright Nickel Salt Nickel Additive 512/502 Nickel brightener 5047 Temperature pH Cathode current density |
350-375 g/l 10 ml/l 0.3-0.6 ml/l 55-60°C 4.6-5.1 3-4 A/dm² |
Produces mirror bright finish on mild steel and stainless steel. EXTRA high levelling brightener system. |
NICKEL BRIGHTENER SUPRA |
Bright Nickel Salt Nickel Additive SUPRA-602 Nickel brightener SUPRA -601 Temperature pH Cathode current density |
350-375 g/l 10 ml/l 0.1-0.3 55-60°C 4.6-5.1 3-4 A/dm² |
Produces bright and white finish specially used for barrel plating parts. Gives very fast lcd coverage with high tolerance to metallic impurities. |
NICKEL BRIGHTENER 5047 |
Concentration | 0.1-0.3 ml/l | Produces ultra bright & high levelled finishing with a whitish colour specially used for steel parts to be plated with chrome as it makes the chrome more bluish. |
NICKEL PURIFIER | Nickel Purifier 400 (liquid) | An Ultimate product which gives tolerance to impurities of copper& Zinc in nickel bath & reduces the use of dummying organic impurities & excess brighteners. | |
SPECIAL SEQUESTRANT 202 and SEQUESTRANT 609 | 0.2-0.5g/l | High quality impurity sewover to be improvers whitness & Lep aera in hideposits. | |
NICKEL LEVELLER 540 |
Nickel leveller 540 | 0.1-0.2 ml/l | Optional extra levelling agent for nickel baths to achieve faster levelling on Steel parts |
BLACK NICKEL SALT BS-63 |
Black Nickel Salt Temperature pH ( Use ammonia) Current Density |
150-200 g/l 40-50°C 4.5-5.1 0.1-1 A/dm² |
Used to produce black colour finish mostly used for decorative articles, jewellery etc. |
BLACK ANTIQUE SALT | Black Antique Salt Temperature pH (Use ammonia) Current Density |
100-150 g/l 40-50°C 4.5-5.1 0.1-1 A/dm² |
Used to produce black brushed colour finish mostly used for decorative articles, Hardware etc. |
SEMI BRIGHT NICKEL | BRIGHT NICKEL SALT NICKEL SB ADDITIVE NIKCEL SB WETTING AGENT Temperature pH Cathode Current Density |
350-375 g/l 1-2 ml/l 0.1-0.3 ml/l 55-60°C 4.6-5.1 3-4 A/dm² |
Semi Bright Nickel process is used to increase the corrosion resistance of mainly steel components used in Automobiles parts. The brightner system gives a potential difference of 120 to 160 mv between the semi bright and bright layer. The single brightner system is very high levelling and easy to control. |
GREY NICKEL
Process | Compositions& Operating Conditions | Applications & Features | |
ANTHRACITE/ BLUE BLACK NICKLE | Nickel Chloride Part - 1 Part - 2 Part - 3 Part - 4 Temperature pH (Use part -2 or HCL) Current Density Cathode rod movement |
170 g/l 65 ml/l 40 ml/l 135 ml/l 15 ml/l 60-70°C 5.0-5.5 0.1-1 A/dm² required |
Produces light grey nickel plating on nickel plated articles.The plating is hard and used on jewellery, sanitary articles and spectacles. Colour can be varied from light grey to dark grey |
ALKALINE GREY NICKEL | GREY NICKEL Conc.-NT-32 GREY NICKEL ADD. NT-33 GREY NICKEL ADDITIVE NT-34 Temperature pH Current Density Cathode rod movement |
200 -250 ml/l TECH. DATA TECH. DATA 50-60°C ALKALINE 0.1-1 A/dm² required |
Produces bluish black bright finish on nickel plated articles. The plating is hard and used on jewellery, sanitary articles and spectacles. Colour can be varied from light grey to dark grey. NT-33 can be used optionally to lighten the color and improve brightness. |
SATIN NICKEL
Process | Compositions& Operating Conditions | Applications & Features | |
SATIN NICKEL PROCESS SN-239 GIVES A COARSE GRAIN DEPOSIT SN-439 GIVES A VERY FINE GRAIN DEPOSIT | Satin Nickel Salt Satin Nickel Additive 35 Satin Nickel Additive 36 Satin Nickel Additive 239/439 pH Density Temperature Cathode current Anode current Cathode rod movement |
500-525 g/l 12-15 ml/l 4-6 ml/l 0.4-0.6 ml/l 4.0-4.4 31-33°BE 55-65°C 4-8 A/dm² 1-3 A/dm² required |
Produces a non glaring silky effect the satinising effect can be varied by varying the concentration of additive 239/439 pH should be increased only by nickel carbonate minimum time required for satin effect is 5 minutes and can be increased upto 15 minutes for extra grain size. |
NICKEL ACTIVATION
Process | Compositions& Operating Conditions | Applications & Features | |
NICKEL ACTIVATION | Concentration Dipping only |
250 ml/l 1 min. |
Used to activate passivated nickel articles for gold or any other decorative finish. |