PROCESS FOR ALUMINIUM
Process | Compositions& Operating Conditions | Applications & Features | |
ALBOND DIP AL - 44 CYANIDE BASED |
Concentration Temperature Time |
250-400 ml/l Room 1-2 mins. |
Produces a light grey deposit on aluminium a nickel strike is recommended after This dip works for better adhesion. |
ALU TONE | Conc Temp Time PH |
220-300ml/1 25-40 °C 30 sec- 1 min Acidic |
To be used on aluminium pieces before albond dip gives a very smooth micro etching to give a very good adhesion of albond dip. |
ALUMON-D BY DIPPING |
Concentration Temperature Time |
250-500 ml/l 25-40°C 1-2 mins |
Non cyanide copper based coating to improve the adhesion of plating on Aluminium. |
ACIDIC MATT ALUMINIUM FINISH BY DIPPING |
Concentration Temperature Time |
100-200 ml/l 20-30°C 1-2 mins |
Produces a white matt finish on Aluminium surface. |
ALKALINE MATTING FOR ALUMINIUM |
Powder Concentration Temperature Time |
80-100 g/l 60-70°C 3-5 mins |
Gives a uniform matt finish on Aluminium before anodizing. |